Discover premium surfactants for various applications. Reliable export services, competitive prices, and high performance guaranteed.
PRODUCT PARAMETERS
Description
Overview of Copper Plate
A copper plate is a flat sheet made from copper or copper alloys, widely used in various industries including electrical, construction, and decorative arts. Known for its excellent conductivity, corrosion resistance, and aesthetic appeal, copper plates are versatile materials suited for numerous applications.
Features of Copper Plate
High Electrical Conductivity: Exceptional ability to conduct electricity, making it ideal for electrical components.
Corrosion Resistance: Resists corrosion and oxidation, ensuring long-lasting performance.
Thermal Conductivity: Efficient in conducting heat, useful in heat exchangers and cookware.
Malleability and Ductility: Can be easily shaped into complex forms without breaking.
Antimicrobial Properties: Naturally resists bacterial growth, beneficial in medical and food industries.
Aesthetic Appeal: Offers a unique color and finish, enhancing architectural and artistic projects.
Specifications of Superalloy Beryllium Copper Bronze C17500 Sheet/Plate
Superalloy Beryllium Copper Bronze C17500 Sheet/Plate– Key Specifications
Product Make-up
C17500 is a high-performance copper alloy. It consists of about 0.4– 1.2% beryllium and as much as 0.2% cobalt or nickel. The rest is mainly copper. This mix gives the product strong mechanical properties and great electric conductivity.
Mechanical Qualities
Tensile stamina: 50,000– 85,000 psi (depending on mood).
Return stamina: 20,000– 70,000 psi.
Prolongation: 5– 30%, which reveals great ductility.
The alloy can be heat-treated to reach peak solidity and strength. After aging, it preserves stability under anxiety and heats.
Physical Attributes
Thickness: 8.25 g/cm TWO.
Melting factor: around 1,000 ° C (1,832 ° F).
Electric conductivity: 22– 48% IACS.
Thermal conductivity: 60– 90 W/m · K.
These attributes make C17500 suitable for components that need both toughness and warmth or electrical energy transfer.
Rust Resistance
C17500 withstands deterioration well in many settings. It stands up versus seawater, commercial atmospheres, and some chemicals. It likewise avoids stress and anxiety deterioration splitting far better than many various other copper alloys.
Typical Applications
This alloy is made use of where reliability issues. Instances include electrical adapters, springs, diaphragms, fasteners, and plastic mold and mildew inserts. It’s also found in aerospace elements, oil and gas devices, and welding devices.
Readily Available Kinds and Tolerances
C17500 sheet and plate are available in various densities– from 0.010 inches up to 3 inches. Sizes and lengths adhere to common mill sizes. Surface surfaces include mill coating, polished, or custom options. Flatness and thickness tolerances satisfy ASTM B194 standards.
Applications of Superalloy Beryllium Copper Bronze C17500 Sheet/Plate
Applications of Superalloy Beryllium Copper Bronze C17500 Sheet/Plate
High-Performance Material for Demanding Environments
C17500 beryllium copper bronze sheet and plate supply an uncommon mix of toughness, conductivity, and durability. This material stands apart where routine copper alloys fall short. It withstands wear, stands up under anxiety, and performs power well. These attributes make it perfect for hard industrial jobs.
Electrical and Electronic Components
Suppliers utilize C17500 in adapters, buttons, and relay parts. Its high electrical conductivity makes sure reputable signal circulation. At the exact same time, its mechanical toughness avoids deformation throughout repeated usage. This equilibrium is tough to find in other steels.
Aerospace and Protection Solutions
In airplane and protection equipment, reliability is non-negotiable. C17500 sheets are utilized in touchdown gear bushings, actuator parts, and fasteners. The alloy handles severe temperatures and heavy loads without failing. It likewise withstands corrosion from fuels, oils, and salt air.
Plastic Mold And Mildew Tooling
Mold makers pick C17500 plates for injection mold and mildews. The product transfers warmth quickly, which quickens cooling down cycles and boosts production rates. Its hardness decreases surface area wear, so molds last longer and maintain fine information over countless cycles.
Oil and Gas Tools
Downhole devices and valves in oil fields deal with rough conditions. C17500 executes well below due to the fact that it will not spark– vital in eruptive settings. It likewise holds up against high stress and withstands sulfide tension fracturing.
Industrial Equipment
Gears, bearings, and use plates made from C17500 run smoother and last longer. The alloy’s reduced friction and high fatigue resistance cut downtime and upkeep expenses. Factories depend on it for components that have to function continuously under load.
This superalloy bridges the gap between pure copper’s conductivity and steel’s toughness. Designers specify it when failing is not a choice.
Company Introduction
Welcome to Wgraj, a premier global supplier of high-quality metal cladding solutions. We specialize in providing a wide range of metal cladding products, including aluminum, steel, and copper composites, designed to meet the diverse needs of architects, builders, and designers. Our commitment to innovation, durability, and aesthetic excellence ensures that our clients receive top-tier materials for their projects. With state-of-the-art manufacturing facilities and a dedication to customer satisfaction, we deliver reliable, cost-effective solutions worldwide. Partner with us for your metal cladding needs and experience unmatched quality and service.
If you have any questions, please feel free to contact us(nanotrun@yahoo.com).
Payment Methods
T/T, Western Union, Paypal, Credit Card etc.
Shipment Methods
By air, by sea, by express, as customers request.
5 FAQs of Superalloy Beryllium Copper Bronze C17500 Sheet/Plate
What is C17500 Beryllium Copper Sheet?
C17500
C17500 is a high-strength copper alloy. It contains beryllium and cobalt or nickel. This mix gives it excellent electrical and thermal conductivity. It also keeps good strength at high temperatures. People use it where both strength and conductivity matter.
Why choose C17500 over other copper alloys?
Better balance of properties
C17500 offers higher strength than regular copper. At the same time, it conducts electricity almost as well as pure copper. Other alloys may be stronger but lose too much conductivity. C17500 strikes the right balance for many industrial uses.
Where is C17500 sheet commonly used?
Key applications
You’ll find C17500 in electrical connectors, springs, and switch parts. It’s also used in plastic molds and welding equipment. Any place needing wear resistance, strength, and good heat transfer can benefit from this material.
Is C17500 easy to machine and form?
Workability
Yes. In its soft (annealed) state, C17500 can be bent, stamped, or formed without cracking. After shaping, it can be heat-treated to reach full strength. Machining is straightforward with standard tools, though sharp cutters work best.
Does C17500 resist corrosion?
Durability in harsh environments
C17500 resists corrosion well. It holds up in seawater, industrial atmospheres, and many chemicals. This makes it reliable for long-term use outdoors or in tough operating conditions. Its surface stays stable without heavy maintenance.