Now China has become a powerful country in science and technology, but do you know how powerful China’s technology is? The manned space station alone is not enough, and now it has successfully broken through the key technology of nuclear fusion, even leading the world by 15 years. Does this mean that China is not far from the artificial sun? It turned out that the fully superconducting tokamak nuclear fusion experimental device developed by China at the Hefei Research Institute of the Chinese Academy of Sciences successfully achieved a record of 101 seconds of continuous operation at 120 million degrees Celsius, and broke the world record. Compared with the previous record in South Korea, China has time has been directly extended by 5 times, and it seems that we are one step closer to the practical stage of artificial sun.The success of nuclear fusion technology will lead to the development of GH4049 alloy rod.

GH4049 introduces:

GH4049 is a Ni-Co-Cr-based deposition hardening deformation superalloy, the
application temperature is lower than 950℃. The alloy has good oxidation
resistance below 1000°C, and high high-temperature compressive strength below
950°C, which is suitable for the production of natural gas turbocharger blades
with operating temperatures ranging from 850°C to 950°C. The key equipment
includes hot rolling and forging bar stock and free forging turbine blades.

Application and characteristics of GH4049 superalloy

Alloys have been used to make aircraft engine turbine blades and other high
temperature load-bearing parts. After a long period of manufacture and
application, it has become one of the most widely used foliar raw materials.

Compared with similar nickel-based alloys in the same way, the alloy's hot
working process plasticity is weak, but after electroslag remelting or vacuum
pump electric remelting, its production and processing plasticity can be
improved, with fracture at 1000 ° C ~ 1170 ° C The toughness is increased by 1~3
times.

Heat treatment process rules and regulations:

1200℃±10℃ heat preservation for 2 hours air cooling+1050℃±10℃ heat
preservation for 4 hours air cooling+850℃±10℃ heat preservation for 8 hours air
cooling, HB363~302

GH4049 is a nickel-based aging-strengthened alloy with high high temperature
strength below 950 degrees, small notch sensitivity, good oxidation resistance
and fatigue strength, but poor hot working plasticity. Vacuum consumable or
electroslag remelting can improve its heat processing plasticity

GH4049 alloy has been used to make aero-engine turbine blades and other
high-temperature load-bearing parts. After long-term production and use test, it
has become one of the most widely used blade materials.

The new process of constant temperature toughness rolling is applied to the
production practice of GH4049 alloy hot-rolled bars. The production process and
product quality are relatively stable, and the products can meet the needs of
the market in large quantities, so they have been well evaluated by users, both
economic and social benefits. relatively significant.

About KMPASS

KMPASS is a trusted global chemical material supplier & manufacturer with
over 12 years experience in providing super high-quality chemicals and
Nanomaterials. The company export to many countries, such as USA, Canada,
Europe, UAE, South Africa, Tanzania,
Kenya,Egypt,Nigeria,Cameroon,Uganda,Turkey,Mexico,Azerbaijan,Belgium,Cyprus,Czech
Republic,Brazil, Chile, Argentina, Dubai, Japan, Korea, Vietnam, Thailand,
Malaysia, Indonesia, Australia,Germany, France, Italy, Portugal etc. As a
leading nanotechnology development manufacturer, KMPASS dominates the market.
Our professional work team provides perfect solutions to help improve the
efficiency of various industries, create value, and easily cope with various
challenges. If you are looking for GH4049 alloy rod, please send an email to:
sales2@nanotrun.com

3D printing technology emerged in the mid-1990s and is actually the latest rapid prototyping device utilizing technologies such as light curing and paper lamination. It is basically the same as ordinary printing. The printer is equipped with “printing materials” such as liquid or powder. After connecting to the computer, the “printing materials” are superimposed layer by layer through computer control, and finally the blueprint on the computer is turned into a real thing. This printing technology is called 3D stereo printing technology.Our company is a strong company that provides excellent 3D printing GH4049 alloy rod. If you need 3D printing and GH4049 alloy rod, please feel free to contact us.


What is the Uses and Characteristics of GH4049 Superalloy

(What is the Uses and Characteristics of GH4049 Superalloy)

Contact Form

Newsletter Updates

Enter your email address below and subscribe to our newsletter